UNS S34700|1.4550|TP347 Seamless Stainless Steel Pipe
Distinguished by the strategic addition of Niobium (Columbium), our TP347 tubing prevents chromium carbide precipitation during prolonged exposure to temperatures in the 427°C - 816°C (800°F - 1500°F) range. This makes them indispensable for mission-critical applications in chemical reactors, high-pressure steam systems, and furnace components. Through advanced cold-drawing and precise solution annealing, XinZhe ensures every pipe maintains a uniform microstructure and optimized mechanical strength for the most aggressive industrial media.
“Our precision-controlled Niobium-to-Carbon ratio ensures that carbides are fully stabilized, preventing sensitization even during welding.”
What Is Seamless Stainless Steel TP347 Pipe?
Stainless Steel 347 Pipe is a cylindrical tube crafted from a single, solid billet of stainless steel. Like other seamless products, it has no weld joint, ensuring maximum structural integrity and high-pressure ratings.
The"347"designation signifies an austenitic stainless steel that is stabilized with the addition of niobium and tantalum. While a low-carbon grade like 304L is excellent for preventing intergranular corrosion during welding, it can still be vulnerable to"sensitization"(carbide precipitation) if exposed to high temperatures for a long time. The niobium/tantalum in 347 binds with carbon, preventing chromium from forming carbides at the grain boundaries. This stabilization ensures that the pipe maintains its superior corrosion resistance even after being exposed to high temperatures up to 870°C (1600°F).
Key Features and Advantages
Stainless Steel 347 Seamless Pipe offer a unique combination of benefits that make them invaluable in demanding applications:
Exceptional Resistance to Intergranular Corrosion
The addition of niobium/tantalum prevents carbide precipitation during welding and high-temperature service. This is the primary advantage, ensuring the material retains its corrosion-fighting properties in the weld zone and throughout its service life.
Superior High-Temperature Performance
It provides better high-temperature strength and creep resistance than 304 stainless steel, making it suitable for a wide range of thermal applications.
Excellent Corrosion Resistance
It offers good general corrosion resistance, similar to 304, in various atmospheric and chemical environments.
High Pressure Tolerance
The seamless construction provides a uniform, robust structure that safely handles high internal pressures.
Product Specifications and Data
To provide a comprehensive overview of this high-performance material, here are the detailed technical specifications and performance data for 347 stainless steel.
Chemical Composition
The key to TP347 's performance is its precise composition, including the crucial addition of niobium/tantalum.
| Grade | C | Cr | Ni | Mn | P | S | Si | Others |
|---|---|---|---|---|---|---|---|---|
| 347 | ≤0.08 | 17.00-19.00 | 9.00-13.00 | ≤2.00 | ≤0.045 | ≤0.030 | ≤0.75 | Nb ≥ 10×C, ≤ 1.00 |
| 347H | 0.04-0.10 | 17.00-19.00 | 9.00-13.00 | ≤2.00 | ≤0.045 | ≤0.030 | ≤1.00 | Nb≥8*C% |
Typical Mechanical Properties
Grade TP347 offers a balance of strength and ductility, making it a reliable solution for various industrial applications.
| Grade | Yield strength ksi(MPa) | Tensile Strength ksi(MPa) | Elongation % | Hardness Brinell/Vickers | Hardness Rockwell |
|---|---|---|---|---|---|
| 347 | ≥30(205) | ≥75(515) | ≥35 | ≤ 192 HBW/200HV | ≤ 90HRB |
| 347H | ≥30(205) | ≥75(515) | ≥35 | ≤ 192 HBW/200HV | ≤ 90HRB |
Typical Physical Properties of TP347 Stainless Steel
These physical properties highlight the material's ability to perform reliably across a range of environments.
| Density | Melting Point | Thermal Expansion | Thermal Conductivity | Modulus of Elasticity | Electrical Resistivity |
|---|---|---|---|---|---|
| 8.0 g/cm³ | 1398 - 1454 °C | 16.6 µm/m·°C (20-100°C) | 16.3 W/m·K (20°C) | 193 GPa | 0.72 x 10⁻⁶ Ω·m (20°C) |
Size Tolerance Chart
| Standard | OD(D) | Tolerance ( MM) | Thickness(S) | Tolerance(MM) | Length | Tolerance | |
| MM | Common | High | MM | MM | |||
| ASTM A312 | D ≤ 48.3 | +0.4/-0.8 | 10.3 ≤ 73 | +20%-12.5% | +6.0/0 | ||
| 48.3 ≤ 114.30 | ±0.8 | 88.9 ≤ 457.2,t/D ≤ 5% | +22.5%/-12.5% | ||||
| 114.3 ≤ 219.1 | +1.6/-0.8 | 88.9 ≤ 457.2,t/D >5% | +15%/-12.5% | ||||
| 219.1 ≤ 457.2 | +2.4/-0.8 | D ≥ 508, t/D ≤ 5%,SMLS | +22.5%/-12.5% | ||||
| 457.2 ≤ 660.4 | +3.2/-0.8 | D ≥ 508, t/D>5%,SMLS | +15%/-12.5% | ||||
| 660.4 ≤ 863.6 | +4.0/-0.8 | D ≥ 508, WELD | +17.5%/-12.5% | ||||
| 863.6 ≤ 1219.2 | +4.8/-0.8 | ||||||
| JIS 3459 Hot-Finished Smls Pipe | D < 50 | ±0.51 | S < 4 | ±0.5 | |||
| D ≥ 50 | ±1.0% | S ≥ 4 | ±12.5% | ||||
| JIS 3459 Cold-Finished | D < 30 | ±0.3 | S < 2 | ±0.2 | |||
| D ≥ 30 | ±1.0% | S ≥ 2 | ±10.0% | ||||
| JIS G3463 Hot-Finished Smls Pipe | 100 | +0.4/-0.8 | D < 100 , S | / | D | +7/0 | |
| D < 100 , 2 ≤ S | +40%/0 | D | +10/0 | ||||
| D < 100 , 2.4 ≤ S | +35%/0 | ||||||
| D < 100 , 3.8 ≤ S | +33%/0 | ||||||
| D < 100 , 4.6 ≤ S | +28%/0 | D | +13/0 | ||||
| 100 ≤ D | +0.4/-1.2 | D>100, S < 2 | / | ||||
| 120 ≤ D | D>100 , 2 ≤ S | / | D | +15/0 | |||
| 160 ≤ D | +0.4/-1.8 | D>100 , 2.4 ≤ S | +35%/0 | ||||
| 200 ≤ D | +0.4/-2.4 | D>100 , 3.8 ≤ S | +33%/0 | D>50,7 | +10/0 | ||
| D>100 , 4.6 ≤ S | +28%/0 | ||||||
| JIS G3463 Cold-finished | +0.4/-0.8 | D | +0.4/0 | ||||
| 60 ≤ D | ±0.3 | D ≥ 2.0 | +20%/0 | D>50,7 | +13/0 | ||
| 80 ≤ D | ±0.4 | D ≥ 40 | +22%/0 | ||||
| 100 ≤ D | +0.4/-0.6 | ||||||
| 120 ≤ D | +0.4/-0.8 | D>50,10M | +15/0 | ||||
| 160 ≤ D | +0.4/-1.2 | ||||||
| 200 ≤ D | +0.4/-1.6 | ||||||
| GB/T 14975 冷拔 ( 扎 ) 钢管 | D | ±0.3 | ±0.1 | 所有壁厚,普通级 PA | +12.5%/-10% | ||
| 12.7 | ±0.15 | ||||||
| 38.1 | ±0.4 | ±0.3 | |||||
| 88.9 | ±0.9% | ±0.4 | |||||
| 139.7 | ±0.8 | 所有壁厚,高级 PC | ±10% | ||||
| 203.2 | ±1.1 | ||||||
| 219.1 | ±1.6 | ||||||
| D ≥ 323.9 | ±0.5% | ||||||
| GB/T 14976 冷拔 ( 轧 ) 钢管 | 6 | ±0.2 | ±0.15 | S ≤ 3 | ±12%(10% /0 高级 PC) | ||
| 10 ≤ D | ±0.2 | ±0.2 | |||||
| 30 ≤ D | ±0.2 | ±0.3 | S>3 | +12.5%/-10%(10%/0 高级 PC) | |||
| 50 ≤ D | 0.85% | 0.75% | |||||
| D>219 | 0.9% | 0.8% | Smin, all | +22%/0(+20%/0 高级 PC) | |||
Common Applications
The combination of superior corrosion resistance and high-temperature stability makes TP347 stainless steel seamless pipes a preferred choice for:
Aerospace
Used in jet engine parts, exhaust manifolds, and afterburners due to its high-temperature strength.
Chemical Processing
In systems handling corrosive chemicals and gases at high temperatures.
Thermal Oxidizers and Boilers
For components that are exposed to high heat and corrosive conditions.
Food Processing
In environments where cleanliness is crucial and piping is exposed to heat.
Manufacturing Process
The manufacturing of a TP347 seamless pipe is a precise, multi-step process:
This meticulous process ensures that every 347 seamless pipe meets the highest standards for performance and reliability in the most demanding applications.
| Test Items of Common Products Standards | ||||||||||||||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Standard | chemistry | stretch | Impact test | flatten | spin over | curve | hardness | Corrosion test | Metallographic examination | ET | UT | HT | size | facade | Remark | |||||
| -196 | tempe- rature | interg- ranular | Point corrosion | Inclusions | grain size | ferr- olites | ||||||||||||||
| GB/T 14976-2012 | √ | √ | X | X | X | X | X | X | √ | X | X | X | X | X | X | √ | √ | √ | HT can be replaced by ET or UT | |
| GB 13296-2013 | √ | √ | X | X | √ | √ | X | X | √ | X | X | X | X | X | √ | √ | √ | √ | HT can be replaced by ET | |
| GB 5310-2008 | √ | √ | X | √ | √ | X | √ | √ | X | X | √ | √ | X | X | √ | √ | √ | √ | ||
| GB 9948-2013 | √ | √ | X | √ | √ | √ | X | √ | √ | X | X | X | X | X | √ | √ | √ | √ | HT can be replaced by ET or MFL | |
| ASTMA312 | √ | √ | X | X | √ | X | X | X | X | X | X | X | X | X | X | √ | √ | √ | HT can be replaced by ET or UT | |
| ASTMA213 | √ | √ | X | X | √ | √ | X | √ | X | X | X | √ | X | X | √ | √ | √ | √ | HT can be replaced by ET | |
| ASTMA269 | √ | √ | X | X | √ | √ | X | √ | X | X | X | X | X | X | X | √ | √ | √ | HT can be replaced by ET or UT | |
| JISG3459 | √ | √ | X | X | √ | X | X | X | X | X | X | √ | X | X | X | √ | √ | √ | HT can be replaced by ET or UT | |
| JISG3463 | √ | √ | X | X | √ | √ | X | X | X | X | X | √ | X | X | X | √ | √ | √ | HT can be replaced by ET or UT | |
| DN 17456 | √ | √ | X | X | X | X | X | X | X | X | X | X | X | X | X | √ | √ | √ | ||
| DN 17458 | √ | √ | X | X | √ | √ | X | X | X | X | X | X | X | X | √ | √ | √ | √ | Flattening or flaring | |
| GB/T 21833.1-2020 | √ | √ | X | X | √ | √ | X | √ | √ | √ | X | X | √ | √ | √ | √ | √ | √ | HT can be replaced by ET or UT | |
| GB/T 21833 2-2020 | √ | √ | X | X | √ | X | X | √ | √ | √ | X | X | √ | √ | √ | √ | √ | √ | HT can be replaced by ET or UT | |
| ASTMA790 | √ | √ | X | X | √ | X | X | √ | X | X | X | X | X | X | √ | √ | √ | √ | HT can be replaced by ET or UT | |
Heating
A solid steel billet is heated to a high temperature.
Piercing
A piercing mill pushes a mandrel through the center of the heated billet to form a hollow shell.
Rolling and Sizing
The hollow shell is then rolled and drawn to reduce its diameter and wall thickness to the desired dimensions.
Finishing
The pipe is cut to length, heat-treated, and subjected to finishing processes like pickling to achieve its final state.
Ready to Request a Quotation?
Send your Seamless Stainless Steel TP347 Pipe enquiry with grade, applicable ASTM/ASME standard and edition, OD × wall thickness, length, quantity, end finish, delivery destination and inspection documents — you will get a written quotation stating the specification and edition, delivery condition, documents included and lead time.